Completed filament profiles: - PETG: Original (240°C, 12mm³/s) & Bambu (245°C, 18mm³/s) - ABS: Original (250°C, 12mm³/s) & Bambu (255°C, 18mm³/s) - TPU: Original (225°C, 8mm³/s) & Bambu (230°C, 10mm³/s) - Carbon Fiber: Bambu ONLY (215°C, 15mm³/s, abrasive!) Key settings per material: - PETG: Lower fan (30%), slower retracts to prevent oozing - ABS: No fan, enclosure required, higher temps - TPU: Very slow retracts (20-25mm/s), minimal retraction - Carbon: Abrasive flag set, steel nozzle required All profiles include: - Correct max volumetric speeds - Temperature offsets for steel nozzle (+5°C) - Shorter retracts for Bambu hotend (1.8mm vs 2.5mm) - Appropriate Pressure Advance values - Filament-specific cooling settings
5.3 KiB
5.3 KiB
🎯 Orca Slicer Profiles - Neptune 4 Plus Dual Hotend
📁 Profil-Struktur
orca-profiles/
├── Neptune4Plus-Original/ # Elegoo Original Hotend (15 mm³/s)
│ ├── process_original.json
│ ├── filament_pla_original.json
│ ├── filament_petg_original.json (TODO)
│ ├── filament_abs_original.json (TODO)
│ └── filament_tpu_original.json (TODO)
└── Neptune4Plus-Bambu/ # Bambu Lab Hotend (23 mm³/s, Steel Nozzle)
├── process_bambu.json
├── filament_pla_bambu.json
├── filament_petg_bambu.json (TODO)
├── filament_abs_bambu.json (TODO)
├── filament_tpu_bambu.json (TODO)
└── filament_carbon_bambu.json (TODO - nur Bambu!)
🔧 Hauptunterschiede
| Setting | Original | Bambu | Warum? |
|---|---|---|---|
| Max Volumetric Speed | 15 mm³/s | 23 mm³/s | Bambu Hotend kann mehr Flow |
| Retract Length | 2.5mm | 1.8mm | Bambu hat kürzere Heatbreak |
| Retract Speed | 35 mm/s | 45 mm/s | Bambu verträgt schnelleres Retract |
| Nozzle Temp (PLA) | 205°C | 210°C | Stahl leitet Wärme schlechter |
| Pressure Advance | 0.027 | 0.022 | Bambu Hotend braucht weniger PA |
| Travel Speed | 350 mm/s | 400 mm/s | Bambu ermöglicht schneller |
| Perimeter Speed | 100 mm/s | 130 mm/s | Höherer Flow erlaubt schnellere Perimeter |
| Infill Speed | 150 mm/s | 200 mm/s | Bambu Hotend kann mehr |
📋 Installation in Orca Slicer
Option A: Import über GUI
- Orca Slicer öffnen
- File → Import → Import Config(s)...
- JSON-Files auswählen
- Profiles erscheinen in den Dropdowns
Option B: Manuell kopieren
# Linux
cp orca-profiles/Neptune4Plus-Original/* ~/.config/OrcaSlicer/profiles/
cp orca-profiles/Neptune4Plus-Bambu/* ~/.config/OrcaSlicer/profiles/
# Windows
# Kopiere nach: %APPDATA%\OrcaSlicer\profiles\
# macOS
# Kopiere nach: ~/Library/Application Support/OrcaSlicer/profiles/
Option C: Presets Ordner
- Orca Slicer → Settings → Preferences
- "Open Preset Folder" klicken
- JSON-Files dort rein kopieren
- Orca neu starten
🔨 Drucktests empfohlen
1. Temperature Tower (für jedes Hotend + Filament)
- Teste: 195°C, 200°C, 205°C, 210°C, 215°C
- Bambu-Hotend braucht evtl. +5°C wegen Stahl-Nozzle
2. Retraction Test
- Teste: 1.5mm, 1.8mm, 2.0mm, 2.5mm
- Original: Start bei 2.5mm
- Bambu: Start bei 1.8mm
3. Pressure Advance Calibration
# Klipper Console
PRESSURE_ADVANCE_CALIBRATE
# Oder Testdruck: https://github.com/TeachingTech3D/Calibration
- Original: Start bei 0.027
- Bambu: Start bei 0.022
4. Max Flow Rate Test
- Drucke einen Würfel mit 100% Infill
- Erhöhe schrittweise die Geschwindigkeit
- Beobachte Underextrusion
🎯 Filament-spezifische Hinweise
PLA
- Original: 205°C, 15 mm³/s, 2.5mm Retract
- Bambu: 210°C, 23 mm³/s, 1.8mm Retract
PETG
- Original: 240°C, 12 mm³/s, 2.5mm Retract
- Bambu: 245°C, 18 mm³/s, 1.8mm Retract
- ⚠️ PETG mag keine zu kurzen Retracts (oozing!)
ABS
- Original: 250°C, 12 mm³/s, 2.5mm Retract
- Bambu: 255°C, 18 mm³/s, 1.8mm Retract
- 🔥 Enclosure empfohlen!
TPU (Flex)
- Original: 225°C, 8 mm³/s, 1.5mm Retract
- Bambu: 230°C, 10 mm³/s, 1.2mm Retract
- ⚠️ TPU braucht LANGSAME Retracts!
Carbon/Glow (NUR Bambu!)
- Bambu: 215-225°C, 15 mm³/s, 1.8mm Retract
- ⚠️ NIEMALS im Original-Hotend (zerstört Messing-Nozzle!)
- Stahl-Nozzle ist abrasionsfest
📊 PRINT_START Macro Anpassung
Für beide Hotends kannst du das gleiche PRINT_START_NOCCI verwenden, aber:
In Slicer Start-Gcode:
; Für Original Hotend
PRINT_START_NOCCI EXTRUDER_TEMP=[nozzle_temperature] BED_TEMP=[bed_temperature] FILAMENT_TYPE=PLA
; Für Bambu Hotend
PRINT_START_NOCCI EXTRUDER_TEMP=[nozzle_temperature] BED_TEMP=[bed_temperature] FILAMENT_TYPE=PLA
Optional: Zwei verschiedene Macros
Du könntest auch zwei Macros machen:
PRINT_START_ORIGINAL→ konservativerPRINT_START_BAMBU→ aggressiver (höhere Temps, schneller)
🔍 Troubleshooting
| Problem | Original | Bambu |
|---|---|---|
| Underextrusion | Flow zu hoch (>15) | Temp zu niedrig |
| Stringing | Retract erhöhen | Temp reduzieren |
| Heat Creep | Lüfter prüfen | Temp reduzieren, Retract kürzen |
| Poor Layer Adhesion | Temp erhöhen | Temp weiter erhöhen (+10°C) |
| Clogging | Hotend reinigen | Heatbreak tauschen |
✅ Alle Profile erstellt (2026-03-12)
Alle Filament-Profile sind jetzt verfügbar:
- PLA - Original & Bambu ✅
- PETG - Original & Bambu ✅
- ABS - Original & Bambu ✅
- TPU - Original & Bambu ✅
- Carbon Fiber - Bambu ONLY ⚠️ (abrasiv, nur Stahl-Nozzle!)
💡 Tipps
- Immer Backup der aktuellen Profiles vor Änderungen
- Temperature Tower für jedes neue Filament drucken
- Pressure Advance bei Hotend-Wechsel neu kalibrieren!
- Flow Rate realistisch setzen (lieber konservativ)
- Notizen machen welche Settings für welches Filament funktionieren
Created: 2026-03-12
Printer: Elegoo Neptune 4 Plus
Hotends: Original (15 mm³/s) + Bambu Lab (23 mm³/s)
Slicer: Orca Slicer
Firmware: Open4Neptune + Klipper + Cartographer 3D