Completed filament profiles: - PETG: Original (240°C, 12mm³/s) & Bambu (245°C, 18mm³/s) - ABS: Original (250°C, 12mm³/s) & Bambu (255°C, 18mm³/s) - TPU: Original (225°C, 8mm³/s) & Bambu (230°C, 10mm³/s) - Carbon Fiber: Bambu ONLY (215°C, 15mm³/s, abrasive!) Key settings per material: - PETG: Lower fan (30%), slower retracts to prevent oozing - ABS: No fan, enclosure required, higher temps - TPU: Very slow retracts (20-25mm/s), minimal retraction - Carbon: Abrasive flag set, steel nozzle required All profiles include: - Correct max volumetric speeds - Temperature offsets for steel nozzle (+5°C) - Shorter retracts for Bambu hotend (1.8mm vs 2.5mm) - Appropriate Pressure Advance values - Filament-specific cooling settings
164 lines
5.3 KiB
Markdown
164 lines
5.3 KiB
Markdown
# 🎯 Orca Slicer Profiles - Neptune 4 Plus Dual Hotend
|
|
|
|
## 📁 Profil-Struktur
|
|
|
|
```
|
|
orca-profiles/
|
|
├── Neptune4Plus-Original/ # Elegoo Original Hotend (15 mm³/s)
|
|
│ ├── process_original.json
|
|
│ ├── filament_pla_original.json
|
|
│ ├── filament_petg_original.json (TODO)
|
|
│ ├── filament_abs_original.json (TODO)
|
|
│ └── filament_tpu_original.json (TODO)
|
|
└── Neptune4Plus-Bambu/ # Bambu Lab Hotend (23 mm³/s, Steel Nozzle)
|
|
├── process_bambu.json
|
|
├── filament_pla_bambu.json
|
|
├── filament_petg_bambu.json (TODO)
|
|
├── filament_abs_bambu.json (TODO)
|
|
├── filament_tpu_bambu.json (TODO)
|
|
└── filament_carbon_bambu.json (TODO - nur Bambu!)
|
|
```
|
|
|
|
## 🔧 Hauptunterschiede
|
|
|
|
| Setting | Original | Bambu | Warum? |
|
|
|---------|----------|-------|--------|
|
|
| **Max Volumetric Speed** | 15 mm³/s | 23 mm³/s | Bambu Hotend kann mehr Flow |
|
|
| **Retract Length** | 2.5mm | 1.8mm | Bambu hat kürzere Heatbreak |
|
|
| **Retract Speed** | 35 mm/s | 45 mm/s | Bambu verträgt schnelleres Retract |
|
|
| **Nozzle Temp (PLA)** | 205°C | 210°C | Stahl leitet Wärme schlechter |
|
|
| **Pressure Advance** | 0.027 | 0.022 | Bambu Hotend braucht weniger PA |
|
|
| **Travel Speed** | 350 mm/s | 400 mm/s | Bambu ermöglicht schneller |
|
|
| **Perimeter Speed** | 100 mm/s | 130 mm/s | Höherer Flow erlaubt schnellere Perimeter |
|
|
| **Infill Speed** | 150 mm/s | 200 mm/s | Bambu Hotend kann mehr |
|
|
|
|
## 📋 Installation in Orca Slicer
|
|
|
|
### Option A: Import über GUI
|
|
1. Orca Slicer öffnen
|
|
2. File → Import → Import Config(s)...
|
|
3. JSON-Files auswählen
|
|
4. Profiles erscheinen in den Dropdowns
|
|
|
|
### Option B: Manuell kopieren
|
|
```bash
|
|
# Linux
|
|
cp orca-profiles/Neptune4Plus-Original/* ~/.config/OrcaSlicer/profiles/
|
|
cp orca-profiles/Neptune4Plus-Bambu/* ~/.config/OrcaSlicer/profiles/
|
|
|
|
# Windows
|
|
# Kopiere nach: %APPDATA%\OrcaSlicer\profiles\
|
|
|
|
# macOS
|
|
# Kopiere nach: ~/Library/Application Support/OrcaSlicer/profiles/
|
|
```
|
|
|
|
### Option C: Presets Ordner
|
|
1. Orca Slicer → Settings → Preferences
|
|
2. "Open Preset Folder" klicken
|
|
3. JSON-Files dort rein kopieren
|
|
4. Orca neu starten
|
|
|
|
## 🔨 Drucktests empfohlen
|
|
|
|
### 1. **Temperature Tower** (für jedes Hotend + Filament)
|
|
- Teste: 195°C, 200°C, 205°C, 210°C, 215°C
|
|
- Bambu-Hotend braucht evtl. +5°C wegen Stahl-Nozzle
|
|
|
|
### 2. **Retraction Test**
|
|
- Teste: 1.5mm, 1.8mm, 2.0mm, 2.5mm
|
|
- Original: Start bei 2.5mm
|
|
- Bambu: Start bei 1.8mm
|
|
|
|
### 3. **Pressure Advance Calibration**
|
|
```bash
|
|
# Klipper Console
|
|
PRESSURE_ADVANCE_CALIBRATE
|
|
# Oder Testdruck: https://github.com/TeachingTech3D/Calibration
|
|
```
|
|
- Original: Start bei 0.027
|
|
- Bambu: Start bei 0.022
|
|
|
|
### 4. **Max Flow Rate Test**
|
|
- Drucke einen Würfel mit 100% Infill
|
|
- Erhöhe schrittweise die Geschwindigkeit
|
|
- Beobachte Underextrusion
|
|
|
|
## 🎯 Filament-spezifische Hinweise
|
|
|
|
### PLA
|
|
- **Original:** 205°C, 15 mm³/s, 2.5mm Retract
|
|
- **Bambu:** 210°C, 23 mm³/s, 1.8mm Retract
|
|
|
|
### PETG
|
|
- **Original:** 240°C, 12 mm³/s, 2.5mm Retract
|
|
- **Bambu:** 245°C, 18 mm³/s, 1.8mm Retract
|
|
- ⚠️ PETG mag keine zu kurzen Retracts (oozing!)
|
|
|
|
### ABS
|
|
- **Original:** 250°C, 12 mm³/s, 2.5mm Retract
|
|
- **Bambu:** 255°C, 18 mm³/s, 1.8mm Retract
|
|
- 🔥 Enclosure empfohlen!
|
|
|
|
### TPU (Flex)
|
|
- **Original:** 225°C, 8 mm³/s, 1.5mm Retract
|
|
- **Bambu:** 230°C, 10 mm³/s, 1.2mm Retract
|
|
- ⚠️ TPU braucht LANGSAME Retracts!
|
|
|
|
### Carbon/Glow (NUR Bambu!)
|
|
- **Bambu:** 215-225°C, 15 mm³/s, 1.8mm Retract
|
|
- ⚠️ **NIEMALS** im Original-Hotend (zerstört Messing-Nozzle!)
|
|
- Stahl-Nozzle ist abrasionsfest
|
|
|
|
## 📊 PRINT_START Macro Anpassung
|
|
|
|
Für beide Hotends kannst du das gleiche `PRINT_START_NOCCI` verwenden, aber:
|
|
|
|
### In Slicer Start-Gcode:
|
|
```gcode
|
|
; Für Original Hotend
|
|
PRINT_START_NOCCI EXTRUDER_TEMP=[nozzle_temperature] BED_TEMP=[bed_temperature] FILAMENT_TYPE=PLA
|
|
|
|
; Für Bambu Hotend
|
|
PRINT_START_NOCCI EXTRUDER_TEMP=[nozzle_temperature] BED_TEMP=[bed_temperature] FILAMENT_TYPE=PLA
|
|
```
|
|
|
|
### Optional: Zwei verschiedene Macros
|
|
Du könntest auch zwei Macros machen:
|
|
- `PRINT_START_ORIGINAL` → konservativer
|
|
- `PRINT_START_BAMBU` → aggressiver (höhere Temps, schneller)
|
|
|
|
## 🔍 Troubleshooting
|
|
|
|
| Problem | Original | Bambu |
|
|
|---------|----------|-------|
|
|
| **Underextrusion** | Flow zu hoch (>15) | Temp zu niedrig |
|
|
| **Stringing** | Retract erhöhen | Temp reduzieren |
|
|
| **Heat Creep** | Lüfter prüfen | Temp reduzieren, Retract kürzen |
|
|
| **Poor Layer Adhesion** | Temp erhöhen | Temp weiter erhöhen (+10°C) |
|
|
| **Clogging** | Hotend reinigen | Heatbreak tauschen |
|
|
|
|
## ✅ Alle Profile erstellt (2026-03-12)
|
|
|
|
Alle Filament-Profile sind jetzt verfügbar:
|
|
|
|
- [x] PLA - Original & Bambu ✅
|
|
- [x] PETG - Original & Bambu ✅
|
|
- [x] ABS - Original & Bambu ✅
|
|
- [x] TPU - Original & Bambu ✅
|
|
- [x] Carbon Fiber - Bambu ONLY ⚠️ (abrasiv, nur Stahl-Nozzle!)
|
|
|
|
## 💡 Tipps
|
|
|
|
1. **Immer Backup** der aktuellen Profiles vor Änderungen
|
|
2. **Temperature Tower** für jedes neue Filament drucken
|
|
3. **Pressure Advance** bei Hotend-Wechsel neu kalibrieren!
|
|
4. **Flow Rate** realistisch setzen (lieber konservativ)
|
|
5. **Notizen machen** welche Settings für welches Filament funktionieren
|
|
|
|
---
|
|
**Created:** 2026-03-12
|
|
**Printer:** Elegoo Neptune 4 Plus
|
|
**Hotends:** Original (15 mm³/s) + Bambu Lab (23 mm³/s)
|
|
**Slicer:** Orca Slicer
|
|
**Firmware:** Open4Neptune + Klipper + Cartographer 3D
|