Completed filament profiles:
- PETG: Original (240°C, 12mm³/s) & Bambu (245°C, 18mm³/s)
- ABS: Original (250°C, 12mm³/s) & Bambu (255°C, 18mm³/s)
- TPU: Original (225°C, 8mm³/s) & Bambu (230°C, 10mm³/s)
- Carbon Fiber: Bambu ONLY (215°C, 15mm³/s, abrasive!)

Key settings per material:
- PETG: Lower fan (30%), slower retracts to prevent oozing
- ABS: No fan, enclosure required, higher temps
- TPU: Very slow retracts (20-25mm/s), minimal retraction
- Carbon: Abrasive flag set, steel nozzle required

All profiles include:
- Correct max volumetric speeds
- Temperature offsets for steel nozzle (+5°C)
- Shorter retracts for Bambu hotend (1.8mm vs 2.5mm)
- Appropriate Pressure Advance values
- Filament-specific cooling settings
2026-03-12 10:44:24 +00:00

164 lines
5.3 KiB
Markdown

# 🎯 Orca Slicer Profiles - Neptune 4 Plus Dual Hotend
## 📁 Profil-Struktur
```
orca-profiles/
├── Neptune4Plus-Original/ # Elegoo Original Hotend (15 mm³/s)
│ ├── process_original.json
│ ├── filament_pla_original.json
│ ├── filament_petg_original.json (TODO)
│ ├── filament_abs_original.json (TODO)
│ └── filament_tpu_original.json (TODO)
└── Neptune4Plus-Bambu/ # Bambu Lab Hotend (23 mm³/s, Steel Nozzle)
├── process_bambu.json
├── filament_pla_bambu.json
├── filament_petg_bambu.json (TODO)
├── filament_abs_bambu.json (TODO)
├── filament_tpu_bambu.json (TODO)
└── filament_carbon_bambu.json (TODO - nur Bambu!)
```
## 🔧 Hauptunterschiede
| Setting | Original | Bambu | Warum? |
|---------|----------|-------|--------|
| **Max Volumetric Speed** | 15 mm³/s | 23 mm³/s | Bambu Hotend kann mehr Flow |
| **Retract Length** | 2.5mm | 1.8mm | Bambu hat kürzere Heatbreak |
| **Retract Speed** | 35 mm/s | 45 mm/s | Bambu verträgt schnelleres Retract |
| **Nozzle Temp (PLA)** | 205°C | 210°C | Stahl leitet Wärme schlechter |
| **Pressure Advance** | 0.027 | 0.022 | Bambu Hotend braucht weniger PA |
| **Travel Speed** | 350 mm/s | 400 mm/s | Bambu ermöglicht schneller |
| **Perimeter Speed** | 100 mm/s | 130 mm/s | Höherer Flow erlaubt schnellere Perimeter |
| **Infill Speed** | 150 mm/s | 200 mm/s | Bambu Hotend kann mehr |
## 📋 Installation in Orca Slicer
### Option A: Import über GUI
1. Orca Slicer öffnen
2. File → Import → Import Config(s)...
3. JSON-Files auswählen
4. Profiles erscheinen in den Dropdowns
### Option B: Manuell kopieren
```bash
# Linux
cp orca-profiles/Neptune4Plus-Original/* ~/.config/OrcaSlicer/profiles/
cp orca-profiles/Neptune4Plus-Bambu/* ~/.config/OrcaSlicer/profiles/
# Windows
# Kopiere nach: %APPDATA%\OrcaSlicer\profiles\
# macOS
# Kopiere nach: ~/Library/Application Support/OrcaSlicer/profiles/
```
### Option C: Presets Ordner
1. Orca Slicer → Settings → Preferences
2. "Open Preset Folder" klicken
3. JSON-Files dort rein kopieren
4. Orca neu starten
## 🔨 Drucktests empfohlen
### 1. **Temperature Tower** (für jedes Hotend + Filament)
- Teste: 195°C, 200°C, 205°C, 210°C, 215°C
- Bambu-Hotend braucht evtl. +5°C wegen Stahl-Nozzle
### 2. **Retraction Test**
- Teste: 1.5mm, 1.8mm, 2.0mm, 2.5mm
- Original: Start bei 2.5mm
- Bambu: Start bei 1.8mm
### 3. **Pressure Advance Calibration**
```bash
# Klipper Console
PRESSURE_ADVANCE_CALIBRATE
# Oder Testdruck: https://github.com/TeachingTech3D/Calibration
```
- Original: Start bei 0.027
- Bambu: Start bei 0.022
### 4. **Max Flow Rate Test**
- Drucke einen Würfel mit 100% Infill
- Erhöhe schrittweise die Geschwindigkeit
- Beobachte Underextrusion
## 🎯 Filament-spezifische Hinweise
### PLA
- **Original:** 205°C, 15 mm³/s, 2.5mm Retract
- **Bambu:** 210°C, 23 mm³/s, 1.8mm Retract
### PETG
- **Original:** 240°C, 12 mm³/s, 2.5mm Retract
- **Bambu:** 245°C, 18 mm³/s, 1.8mm Retract
- ⚠️ PETG mag keine zu kurzen Retracts (oozing!)
### ABS
- **Original:** 250°C, 12 mm³/s, 2.5mm Retract
- **Bambu:** 255°C, 18 mm³/s, 1.8mm Retract
- 🔥 Enclosure empfohlen!
### TPU (Flex)
- **Original:** 225°C, 8 mm³/s, 1.5mm Retract
- **Bambu:** 230°C, 10 mm³/s, 1.2mm Retract
- ⚠️ TPU braucht LANGSAME Retracts!
### Carbon/Glow (NUR Bambu!)
- **Bambu:** 215-225°C, 15 mm³/s, 1.8mm Retract
- ⚠️ **NIEMALS** im Original-Hotend (zerstört Messing-Nozzle!)
- Stahl-Nozzle ist abrasionsfest
## 📊 PRINT_START Macro Anpassung
Für beide Hotends kannst du das gleiche `PRINT_START_NOCCI` verwenden, aber:
### In Slicer Start-Gcode:
```gcode
; Für Original Hotend
PRINT_START_NOCCI EXTRUDER_TEMP=[nozzle_temperature] BED_TEMP=[bed_temperature] FILAMENT_TYPE=PLA
; Für Bambu Hotend
PRINT_START_NOCCI EXTRUDER_TEMP=[nozzle_temperature] BED_TEMP=[bed_temperature] FILAMENT_TYPE=PLA
```
### Optional: Zwei verschiedene Macros
Du könntest auch zwei Macros machen:
- `PRINT_START_ORIGINAL` → konservativer
- `PRINT_START_BAMBU` → aggressiver (höhere Temps, schneller)
## 🔍 Troubleshooting
| Problem | Original | Bambu |
|---------|----------|-------|
| **Underextrusion** | Flow zu hoch (>15) | Temp zu niedrig |
| **Stringing** | Retract erhöhen | Temp reduzieren |
| **Heat Creep** | Lüfter prüfen | Temp reduzieren, Retract kürzen |
| **Poor Layer Adhesion** | Temp erhöhen | Temp weiter erhöhen (+10°C) |
| **Clogging** | Hotend reinigen | Heatbreak tauschen |
## ✅ Alle Profile erstellt (2026-03-12)
Alle Filament-Profile sind jetzt verfügbar:
- [x] PLA - Original & Bambu ✅
- [x] PETG - Original & Bambu ✅
- [x] ABS - Original & Bambu ✅
- [x] TPU - Original & Bambu ✅
- [x] Carbon Fiber - Bambu ONLY ⚠️ (abrasiv, nur Stahl-Nozzle!)
## 💡 Tipps
1. **Immer Backup** der aktuellen Profiles vor Änderungen
2. **Temperature Tower** für jedes neue Filament drucken
3. **Pressure Advance** bei Hotend-Wechsel neu kalibrieren!
4. **Flow Rate** realistisch setzen (lieber konservativ)
5. **Notizen machen** welche Settings für welches Filament funktionieren
---
**Created:** 2026-03-12
**Printer:** Elegoo Neptune 4 Plus
**Hotends:** Original (15 mm³/s) + Bambu Lab (23 mm³/s)
**Slicer:** Orca Slicer
**Firmware:** Open4Neptune + Klipper + Cartographer 3D